System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Network Polymers Softflex® 0150
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Thermoplastic Elastomer, Melt-Processible Rubber
Material Notes:
Description:
Softflex
®
Thermoplastic Elastomer Alloy
Information provided by Network Polymers Inc.
A. Schulman has acquired Network Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
0.890
g/cc
ASTM D792
Linear Mold Shrinkage, Flow
0.017
cm/cm
@Thickness 3.17 mm
ASTM D955
Linear Mold Shrinkage, Transverse
0.015
cm/cm
@Thickness 3.17 mm
ASTM D955
Melt Flow
150
g/10 min
@Load 1.00 kg,
Temperature 235 °C
Procedure A Condition Q; ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore A
10 - 20
Instantaneous; ASTM D2240
Tensile Strength, Yield
435
psi
chs 20 in/min; ASTM D412
Elongation at Break
800 %
ASTM D412
Gardner Impact
>=
320
in-lb
@Temperature -30.0 °C
ASTM D5420
Tear Strength
8.80
kN/m
ASTM D624
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer
Advanced Elastomer Systems Santoprene® 8281-35W237 Thermoplastic Rubber
Network Polymers Softflex® 0250
Buckeye Polymers BP FLEX A 2305 Soft Touch TPE
Barlog Plastics KEBAFLEX SG 25 A.1 TPE-S, Shore A25, natural
PDIAM000 / 29838
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.