MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Adflex™ KS311P Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin; Polyolefin, Film Grade; Polyolefin, Film Grade (Polyolefin)

Material Notes: Description: Adflex™ KS-311P thermoplastic olefin resin is a barefoot formulation (no slip, no antiblock) designed for cast film extrusion applications. It is based on proprietary Basell process technology KS-311P resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.2600 for rubber articles for repeated use applications. The final item is subject to the extraction requirements in 21 CFR 177.2600. All ingredients in KS-311P resin meet the chemical registration requirements of TSCA (U.S.) and DSL (Canada). Uses: Film, cast, stationary supplies

Information provided by Basell.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.892 g/ccASTM D792
Melt Flow 9.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 56ASTM D2240
Tensile Strength, Yield 2200 psiASTM D 638
Elongation at Break 580 %ASTM D 638
Elongation at Yield 15 %ASTM D 638
Flexural Modulus, 1% Secant 69000 psiProcedure A; ASTM D790
Izod Impact, Notched NB73°F; ASTM D256
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Adflex™ Q 100 F Polyolefin
LyondellBasell Adflex™ KS-021P TPO Resin
LyondellBasell Adsyl™ 5 C 30 F Polyolefin
ExxonMobil EXACT™ 8201 Plastomer for Polymer Modification
ExxonMobil EXACT™ 8201 Plastomer for Blown Film Applications

PMO756 / 53745

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.