Hostacom CR 250 F/M T 8051 is a 16% talc filled impact modified polypropylene, with excellent impact/stiffness balance, good scratch resistance, and UV resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 8051 color version. Applications: Interior Automotive Applications.Information provided by LyondellBasell. |