MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-MASK II HT Conductive Foil Tape
Categories: Polymer; Tape

Material Notes: The CHO-MASK II family of EMI foil tapes includes both Standard Tack (ST) and High Tack (HT) versions for providing a conductive, non-corroding surface on painted metal electronic enclosures. CHO-MASK II tapes consist of recessed polyester paint masking film covering a layer of either 1 oz. (28.4g) or 2 oz. (56.7g) tinplated copper foil. The back of the foil features a conductive pressure sensitive adhesive (PSA). CHO-MASK II tape is applied to clean metal frame, door and panel surfaces where electrical continuity is required. After painting, the peel-off mask is easily removed, allowing the paint to seal both edges of the foil layer. The foil imparts a clean, electrically conductive path from the panel, through an EMI gasket, to the cabinet frame. It also provides grounding points within the enclosure.

Application: Oven bake up to 400°F (204°C) for 1 hour; Suitable for knife edge, radius and flat surface applications; Lengths of <5 ft. above 350°F (177°C) recommended

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.40 mil1 oz. Tinned Copper Foil
 2.00 milAcrylic Adhesive
 2.80 mil2 oz. Tinned Copper Foil
 3.00 mil1 oz. Total Thickness; ASTM D1000
 4.80 mil2 oz. Total Thickness; ASTM D1000
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 0.20 ohmChomerics TM 71
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 82.0 °CChomerics
Minimum Service Temperature, Air -40.0 °CChomerics
 
Processing PropertiesOriginal ValueComments
Cure Time <= 1.00 hour
@Temperature 204 °C
Paint Cure Cycle
 
Descriptive Properties
Adhesion Mask to Foil24 oz./inchASTM D1000
Adhesion to Aluminum543 N/m48 hrs @ 177°C; ASTM D1000
 700 N/m1 hr @ 177°C; ASTM D1000
 718 N/m168 hrs @ 74°C/95% RH; ASTM D1000
 893 N/m1 hr @ 204°C; ASTM D1000
Adhesion to Steel525 N/m48 hrs @ 177°C; ASTM D1000
 683 N/m1 hr @ 177°C; ASTM D1000
 700 N/m168 hrs @ 74°C/95% RH; ASTM D1000
 875 N/m1 hr @ 204°C; ASTM D1000
Chemical ResistancePassTrichloroethane, ethanol, acids, cleaning solvents, and alkaline solutions; ASTM D896-84
Corrosion ResistancePassSalt Fog Chamber at 35°C, 144 hrs; MIL-STD-810
Humidity Exposure Pass@ 60°C for 96 hours 95% RH; ASTM D1001
Mask TypePolyester

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME095 / 28317

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.