MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Hicast HTA Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Andalusite. Bond type: Hydraulic. A low cement, and alusite 1650°C castable with high strengths at all temperatures, low porosity and excellent abrasion, impact and alkali resistance.

Applications:

  • Forge furnace hearths
  • Door jambs, lintels and piers
  • Cartops
  • Rotary kiln nose rings, retainer rings and ams
  • Rotary hearth curbs
  • Walking beam furnace hearth, pusher furnace hearths
  • Skid pipe protection

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramic
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.60 g/ccdried to 110°C
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 80.0 MPa
@Treatment Temp. 110 °C
Cold Crushing Strength
 80.0 MPa
@Treatment Temp. 815 °C
Cold Crushing Strength
 100 MPa
@Treatment Temp. 1000 °C
Cold Crushing Strength
 100 MPa
@Treatment Temp. 1600 °C
Cold Crushing Strength
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.83 W/m-K
@Temperature 600 °C
Maximum Service Temperature, Air <= 1650 °C
Shrinkage -1.50 - 0.00 %
@Treatment Temp. 1600 °C
 0.00 - 0.20 %
@Treatment Temp. 110 °C
 0.20 %
@Treatment Temp. 815 °C
 0.30 %
@Treatment Temp. 1000 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 59 %
CaO 1.6 %
Fe2O3 0.80 %
K2O+Na2O 0.40 %
MgO 0.20 %
SiO2 38 %
TiO2 0.10 %
 
Descriptive Properties
Net Material Required (kg/m³)2600
Water Addition[5.5-6 % by weight, 1.375-1.5 L volume per bag, 25 kg bag weight]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6061 / 202845

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.