MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECASINT 4051 Polyimide, Beige, 30% Glass Fiber (PI)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Glass Fiber

Material Notes: TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excellent wear resistance among other things. The TECASINT 2000 series offers these enhanced thermal properties along with lower moisture absorption, a higher degree of toughness, and better machining properties. TECASINT 2011 is unfilled, while TECASINT 2021 contains 15% graphite which offer improved wear resistance and a lower coefficient of friction. TECASINT 2000 series with their superior physical properties, are ideal for application in the aerospace, nuclear, automotive, electrical/electronics, and chemical processing industries.

Main features: High thermal and mechanical capacity, very creep resistant, high gamma radiation resistance, very low water absorption, good chemical resistance, low coefficient of thermal expansion, easily machined to tight tolerances, very good electrical insulation, flame retardant according to UL94 V-0

Applications: Mechanical engineering, electronics, cryogenics, nuclear and vacuum technology, aircraft and aerospace industries, semiconductor technology, electrical engineering

Preferred Fields: Valve seating, switch parts, insulators, lead backer

Information Provided by Ensinger Sintimid

Key Words: PI GF30
Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.65 g/ccDIN 53 479
Water Absorption 0.060 %
@Temperature 23.0 °C
24 hours in water; EN ISO 62
 0.26 %
@Temperature 80.0 °C
24 hours in water; EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 90
@Temperature 23.0 °C
DIN 53 505
Tensile Strength 77.0 MPa
@Temperature 23.0 °C
EN ISO 527
Elongation at Break 1.2 %
@Temperature 23.0 °C
EN ISO 527
Tensile Modulus 7200 MPa
@Temperature 23.0 °C
EN ISO 527
Flexural Strength 136 MPa
@Temperature 23.0 °C
EN ISO 178
Flexural Modulus 6400 MPa
@Temperature 23.0 °C
EN ISO 178
Flexural Strain at Yield 2.3 %
@Temperature 23.0 °C
EN ISO 178
Compressive Yield Strength 193 MPa
@Strain 10 %,
Temperature 23.0 °C
EN ISO 604
Compressive Strength 259 MPa
@Temperature 23.0 °C
EN ISO 604
Compressive Modulus 2740 MPa
@Temperature 23.0 °C
EN ISO 604
Charpy Impact Unnotched 19.7 kJ/m²
@Temperature 23.0 °C
EN ISO 179
Charpy Impact, Notched 5.00 kJ/m²
@Temperature 23.0 °C
EN ISO 179
Compression Set 42.8 %
@Temperature 23.0 °C
Compression at Break; EN ISO 604
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.80e+16 ohm-cm
@Temperature 23.0 °C
IEC 60093
Surface Resistivity per Square 9.40e+16 ohm
@Temperature 23.0 °C
IEC 60093
Dielectric Constant 3.59
@Frequency 1000 Hz,
Temperature 23.0 °C
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 38.0 µm/m-°C
@Temperature 50.0 - 200 °C
DIN 53 752
 47.0 µm/m-°C
@Temperature 200 - 300 °C
DIN 53 752
CTE, linear, Transverse to Flow 51.0 µm/m-°C
@Temperature 50.0 - 200 °C
DIN 53 752
 70.0 µm/m-°C
@Temperature 200 - 300 °C
DIN 53 752
Thermal Conductivity 0.400 W/m-K
@Temperature 40.0 °C
ISO 8302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger TECASINT 5051 Polyimide, 30% Glass Fiber Filled (PI)
Hippe PI
Ensinger TECASINT 1041 Polyimide, 30% MoS2 Filled (PI)
Ensinger TECASINT 3032 Polyimide, Black, 40% Graphite (PI)
Ensinger TECASINT 4011 Polyimide, Yellow (PI)

PENSIN079 / 121082

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.