MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02)
Categories: Metal; Ferrous Metal; Tool Steel; Oil-Hardening Steel

Material Notes: An oil-hardening alloy with excellent size change properties, Stentor tool steel is especially suited for general purpose work in the toolroom. It is safe to harden, and shows little size change or warpage during the hardening operation. Stentor alloy tool steel is available as a DeCarb-Free product. DCF bars have been cold finished in the mill, eliminating the need for bar bark removal.

Applications: Blanking dies, Forming dies, Lamination dies, Molding dies, Trimming dies, Master tools, Spindles, Master taps, Thread gauges, Collets, Stamps

Information provided by Carpenter Technology Corporation.

Stentor® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS T31502
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 33 - 37Tempered at 1000°F.
 63 - 65As quenched
Tensile Strength, Ultimate 1275 MPawhen tempered around 950°F
Tensile Strength, Yield 1100 MPawhen tempered around 950°F
Elongation at Break 3.0 %when tempered around 950°F
Reduction of Area 16 %when tempered around 950°F
Modulus of Elasticity 209 GPa
Izod Impact Unnotched 120 Jwhen tempered around 600°F
Abrasion 59.5loss in mm3, As-Hardened; ASTM G65
 118.6loss in mm3, Tempered at 875°F; ASTM G65
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µm/m-°C
@Temperature 25.0 - 38.0 °C
 13.3 µm/m-°C
@Temperature 25.0 - 316 °C
 15.1 µm/m-°C
@Temperature 25.0 - 649 °C
Transformation Temperature 727 °CAc1
 749 °CAc3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.90 %
Iron, Fe 97.25 %As Balance
Manganese, Mn 1.6 %
Silicon, Si 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type O2 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 260°C
AISI Type A2 Tool Steel
JIS SKS95M Oil-hardening Cold Work Tool Steel
AISI Type O1 Oil-hardening Tool Steel, oil quenched at 800°C, tempered at 425°C
Carpenter R.D.S.® Alloy Tool Steel (Oil-Hard) (AISI L6)

NCARN15 / 15854

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.