MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BYK Fulcat® 200 Clay Catalyst and Adsorbent
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Fulcat® 200 is a refined natural Montmorillonite clay catalyst and adsorbent. The natural clay structure provides Lewis and Brönsted acid sites that together with a moderate surface area make Fulcat® 200 suitable for acid catalyzed reactions where high levels of acidity are disadvantageous. It is particularly suitable to the dimerisation of Tall Oil fatty acids. Control of clay quality and the clay refining process ensures that Fulcat® 200 provides excellent and reproducible performance

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 69.9 lb/ft³
Particle Size >= 4.0 µm10% less than
 20 - 35 µm50% less than
 <= 90 µm90% less than
Specific Surface Area 100 m²/g
 
Component Elements PropertiesOriginal ValueComments
Al2O3 17 %
Fe2O3 8.1 %
Free Water 8.0 - 14 %
Loss on Ignition(%) 7.0 %
MgO 3.6 %
Na2O 0.40 %
SiO2 58 %
 
Descriptive Properties
Cation Exchange Capacity90 meq/100 g
Pore volume0.1 cm3/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Fulcat® 400 Clay Catalyst and Adsorbent
BYK Cloisite® Ca++ Bentonite
BYK Cloisite® 93A Nanoclay
BYK Cloisite® 93 Salt with bentonite
BYK Cloisite® 5 Salt with bentonite

PBYK045 / 185042

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.