MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Corning Large Cover Gorilla® Glass Touch Screen Glass
Categories: Ceramic; Glass; Optical

Material Notes: Corning® Gorilla® Glass is a damage-resistant cover glass that is elegant, lightweight, and durable enough to resist many real-world events that commonly cause glass failure. The composition of Corning Gorilla Glass allows for a deep layer of high compressive stress (created through an ion-exchange process). This compression acts as a sort of “armor,” making the glass exceptionally tough and damage resistant. Additionally, Corning Gorilla Glass is formed using the same proprietary fusion process as all of Corning’s high-technology display substrates. This extraordinarily precise, highly automated process produces glass with exceptionally clean, smooth, flat surfaces and outstanding optical quality.

Large Cover Gorilla® Glass is sized to serve as cover glass for displays including interactive white boards, digital signage and other large-size public displays.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.44 g/cc
Thickness 550 - 2000 microns
 
Mechanical PropertiesOriginal ValueComments
Vickers Microhardness 534kgf/mm²; unstrengthened (200 g load)
 649kgf/mm²; strengthened (200 g load)
Modulus of Elasticity 71.7 GPa
Compressive Strength 800 MPaChemically Strengthened, >40 µm layer
Poissons Ratio 0.21
Fracture Toughness 0.700 MPa-m½
Shear Modulus 29.6 GPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 8.45 µm/m-°C
@Temperature 0.000 - 300 °C
Softening Point 852 °C107.6 Poise
Annealing Point 649 °C1013.2 Poise
Strain Point 563 °C1014.7 Poise
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.5094
@Wavelength 633 nm
core glass
 1.5116
@Wavelength 633 nm
compression layer
Transmission, Visible >= 91.5 %
@Wavelength 380 - 780 nm
 >= 92 %
@Wavelength 480 - 730 nm
 
Descriptive Properties
Photo-elastic Constant29.4 nm/cm/MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corning Gorilla® Glass 3 Touch Screen Glass with NDR
Corning Antimicrobial Gorilla® Glass Touch Screen Glass
Corning Gorilla® Glass 2
Corning Gorilla® Glass 4 Touch Screen Glass
Corning Gorilla® Glass 5 Display Glass

CCORNG14h / 178187

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.