System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Haysite 54500 Polyester SMC, 35% Glass Reinforced
Categories:
Polymer
;
Thermoset
;
Composite SMC
;
Filled/Reinforced Thermoset
;
Polyester, TS
;
Thermoset Polyester Glass SMC
Material Notes:
A high strength fiberglass reinforced thermoset polyester compound formulated for injection, compression, or transfer molding. This material exhibits excellent electrical and mechanical properties, and has a UL94 Flame Class V-0.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.70
g/cc
ASTM D572
Water Absorption
0.25 %
ASTM D570
Linear Mold Shrinkage
0.0025
cm/cm
Mechanical Properties
Original Value
Comments
Tensile Strength, Ultimate
128
MPa
Flexural Strength
248
MPa
Compressive Strength
145
MPa
Izod Impact, Notched
12.8
J/cm
edgewise; ASTM D256
Electrical Properties
Original Value
Comments
Dielectric Strength
20.0
kV/mm
Perpendicular (ASTM D149), Short Time
Arc Resistance
185
sec
ASTM D495
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
130
°C
temperature rating
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Haysite 43000 Polyester SMC, 22% Glass Reinforced
Haysite 46000 Polyester SMC, 30% Glass Reinforced
Applied Composites 8057 Polyester SMC
Applied Composites 120 Polyester SMC
Applied Composites 150 Polyester SMC
PHAY13 / 45619
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.