MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.

Key Features and Benefits:

  • Epoxy resin system optimized for use with woven aramid reinforcements
  • Meets requirements of MIL-R-9300B, Type 1
  • Long out-time for easy processing

Applications/Qualifications:

  • Military Helicopters
  • Engine Nacelles
  • Work Platforms
  • Doors
  • Air Frames

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 3.0 %
@Temperature 135 °C
8 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 76000 psi
@Temperature 87.8 °C
0° Direction, Wet (2hr water boil immersion); ASTM D638 Type 1
 79000 psi
@Temperature 93.3 °C
0° Direction, Dry; ASTM D638 Type 1
 81000 psi
@Temperature 23.9 °C
0° Direction, Dry; ASTM D638 Type 1
 81000 psi
@Temperature 87.8 °C
0° Direction, Dry; ASTM D638 Type 1
Tensile Modulus 3800 ksi
@Temperature 93.3 °C
0° Direction, Dry; ASTM D638 Type 1
 3900 ksi
@Temperature 87.8 °C
0° Direction, Wet (2hr water boil immersion); ASTM D638 Type 1
 4000 ksi
@Temperature 87.8 °C
0° Direction, Dry; ASTM D638 Type 1
 4400 ksi
@Temperature 23.9 °C
0° Direction, Dry; ASTM D638 Type 1
Flexural Strength 39.0 ksi
@Temperature 87.8 °C
Wet (2hr water boil immersion); ASTM D790
 40.0 ksi
@Temperature 93.3 °C
Dry; ASTM D790
 43.0 ksi
@Temperature 87.8 °C
Dry; ASTM D790
 50.0 ksi
@Temperature 23.9 °C
Dry; ASTM D790
Flexural Modulus 3300 ksi
@Temperature 93.3 °C
Dry; ASTM D790
 3400 ksi
@Temperature 87.8 °C
Dry; ASTM D790
 3600 ksi
@Temperature 87.8 °C
Wet (2hr water boil immersion); ASTM D790
 3800 ksi
@Temperature 23.9 °C
Dry; ASTM D790
Compressive Strength 18.0 ksi
@Temperature 87.8 °C
Wet (2hr water boil immersion); ASTM D695
 22.0 ksi
@Temperature 87.8 °C
Dry; ASTM D695
 22.0 ksi
@Temperature 93.3 °C
Dry; ASTM D695
 29.0 ksi
@Temperature 23.9 °C
Dry; ASTM D695
Compressive Modulus 3000 ksi
@Temperature 87.8 °C
Wet (2hr water boil immersion); ASTM D695
 3100 ksi
@Temperature 87.8 °C
Dry; ASTM D695
 3200 ksi
@Temperature 93.3 °C
Dry; ASTM D695
 3300 ksi
@Temperature 23.9 °C
Dry; ASTM D695
Shear Strength 4.30 ksi
@Temperature 87.8 °C
Short-Beam, Wet (2hr water boil immersion); ASTM D2344
 4.60 ksi
@Temperature 93.3 °C
Short-Beam, Dry; ASTM D2344
 5.50 ksi
@Temperature 87.8 °C
Short-Beam, Dry; ASTM D2344
 5.60 ksi
@Temperature 23.9 °C
Short-Beam, Dry; ASTM D2344
 
Processing PropertiesOriginal ValueComments
Gel Time 1.00 - 4.00 min
Shelf Life 12.0 Month
@Temperature -17.8 °C
 
Descriptive Properties
Prepreg Resin Content (%)52-58
Resin Flow (%)15-35325°F, 15psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont™ Kevlar® 49 Aramid Fiber
Arlon Electronic Materials 45NK Woven Kevlar® Reinforced Laminate and Prepreg
Solvay CYCOM® 950-1 Epoxy Prepreg with 52% 120 Kevlar Fabric
DuPont™ Kevlar® 29 Aramid Fiber
DuPont™ Kevlar® 149 Aramid Fiber, diam. 12 µm

PPARK010 / 89282

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.