MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BEC Materials SEPS 4010
Categories: Polymer; Thermoplastic

Material Notes: Description: Thermoplastic elastomer SEPS (Styrene-Ethylene-Propylene-Styrene) YH-4010 is a powdered, linear SEPS polymer with styrene content of 37% and diblock content of 100%. Lubricant modified by SEP is with lower solution temperature and the higher solution rate.

Application: Fiber Filling Gel

Formula: Fiber filling gel
Hydrogenation mineral oil, NO26, Sinopec: 90g
SEPS YH-4010: 10g

Information provided by BEC Materials, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity >= 500000 cPSolution
Kinematic Viscosity 1800 cSt
@Temperature 80.0 °C
Formula
Kinematic Viscosity at 40°C (104°F) 4500 cStFormula
Melt Flow <= 1.0 g/10 min
 
Chemical PropertiesOriginal ValueComments
Styrene Content 37 %Bound
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore C 80
 
Descriptive Properties
Appearancetransparent
Diblock content1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBECM089 / 307042

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.