MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Engineered Syntactic Systems MZ-32 Deep Water Syntactic Foam
Categories: Polymer

Material Notes: Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having high compressive and hydrostatic strengths. This yields a product able to withstand the high hydrostatic pressures experienced by today’s manned and unmanned subsea vehicles.

The MZ Grade of syntactic safely operates in the oceans Mesopalegic Zone, down to depths of 1,000 meters. (3280 feet). This group of syntactics is produced using the same technology as the Navy’s submarine void filling materials. This workhorse foam system has been thoroughly tested both during development and during its long history in service. It has been found to be a safe, reliable, cost effective buoyancy source for the relatively shallow requirements for a syntactic. Each block is cast as a single unit, but may be cut to fit the application requirement. Blocks or trimmed parts may also be bonded together to form a larger structure.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 30.0 - 34.0 lb/ft³
Water Absorption <= 3.0 %
@Time 86400 sec
at depth
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 2450 psi
Compressive Modulus 160 ksi
Hydrostatic Design Basis 3300 psiHydrostatic Crush Strength
 
Descriptive Properties
Service Depth (feet)3065
Service Pressure (psi)1350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Matrix 999225 Composite Syntactic Foam
Synfoam® AI-42 Syntactic Foam
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 900
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition A

PESS951 / 93173

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.