MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Unifrax IsoMat® AV/AVi Substrate Support Mat
Categories: Ceramic; Oxide; Magnesium Oxide; Silicon Oxide

Material Notes: Developed to meet the most stringent European regulatory requirements, IsoMat AV/Avi is engineered utilizing the unique Isofrax® 1260°C fibers - a green fiber produced using patented magnesia-silicate chemistry.

These fibers are the product of a long-term research and development effort by Unifrax to produce a biosoluble fiber with high-temperature performance characteristics up to 1260°C. Isofrax fibers exhibit excellent chemical stability and resistance to attack from most corrosive agents including combustion by-products of gasoline and diesel fuels.

Mat Performance and Applications: As a manufacturer of fibers used in a variety of catalytic converter mounting systems, Unifrax has successfully combined fiber-making expertise with a state-of-the-art paper manufacturing process to maximize the performance of IsoMat AV/AVi. Like intumescent support mats utilizing traditional ceramic fibers, IsoMat AV/AVi can be designed to provide excellent holding force at continuous operating temperatures up to 900°C inlet gas temperature. Additional holding force is provided by vermiculite particles trapped in a structural support matrix of Isofrax fibers. The fiber matrix provides resistance to hot gas mat erosion. IsoMat AV/AVi expands with increasing relative thickness when first exposed to temperatures in excess of 325°C.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Loss On Ignition >= 6.0 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield >= 0.100 MPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.180 W/m-K
@Temperature 650 °C
ASTM C177
Maximum Service Temperature, Inert 900 °C
 
Descriptive Properties
Binder System (%)8-12
Isofrax® Fibers (%)36-48
Vermiculite (%)42-53

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Rogers Arlon 90B32R016AC Aluminum Clad Press Pad with "C-Finish"
Overview of materials for Polyimide
DuPont Mobility and Materials Kalrez® 6221 FFKM Perfluoroelastomer

CUNIF128 / 97900

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.