MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ MG100 LO Medical Grade Instant Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plastics, rubbers, and composite materials and are available with special properties such as fast cure, low odor, flexibility and a variety of viscosities. This product has been tested and meets the specifications of USP Class VI. These products are not intended for use in implantable medical assemblies or for direct application to the skin. MG100 LO is formulated to have low volatility means that these products are not only low volatility while maintaining bonding of a wide range of materials. Low volatility means that this product is not only low odor but also low blooming. Lower odor can improve worker comfort in applications where assembly requires being close to adhesive dispensing or where ventilation is limited.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/cc
Viscosity 80 - 120 cPU-Tube E40-E43
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14.5 MPacured, grit-blasted steel; ISO 6922
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 71.0 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.167 - 1.00 minTime to Handling
 24.0 hourFull Cure
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
AppearanceClear Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ MG1500 PR Medical Grade Instant Adhesive
3M Scotch-Weld™ MG79 AC Medical Grade Instant Adhesive Primer

PMM34746 / 169493

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.