MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Perstorp Compounds Akestra™ 100 Thermoplastic Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Excellent appearance, clarity, hydrolytic stability, heat resistance and high strength. Used for extrusion and injection molded articles, blow molding, films and sheets. It can be used as a polystyrene alternative for heat resistant thin wall containers, a polycarbonate alternative for durable “dishwasher proof” transparent products, and a glass alternative for hot-fill food containers.

Information provided by Perstorp Compounds Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.27 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 55.0 MPa
Elongation at Break 200 %ASTM D638
Flexural Yield Strength 90.0 MPaASTM D790
Flexural Modulus 2.50 GPaASTM D790
Izod Impact, Notched 25.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 100 °CASTM D7426
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ASTM D1003
Transmission, Visible 91 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik DYNACOLL® 7363 Copolyester
Teknor Apex Terraloy™ BP 20001A Thermoplastic Starch + Copolyester
Perstorp Compounds Akestra™ 90 Thermoplastic Copolyester
Chesterton ARC 988 Composite
BASF Ultramid® C33 PA6/66

PPERST090 / 161710

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.