MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zoltek™ PX35 Pultruded 62% Carbon Fiber/Epoxy Plate
Categories: Polymer; Thermoset; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Pultrusion is a cost-effective, continuous process for producing fiber-reinforced composite parts. ZOLTEK PX35 carbon fiber tows are fed into a proprietary impregnation and curing process which creates engineered carbon fiber profiles. These profiles enable rapid section buildup when laminating thick parts such as wind blade spar caps. High fiber alignment achieved with pultrusion delivers consistently superior properties in laminates compared to any other composite manufacturing processes.

APPLICATIONS: • Wind Energy (pre-cured carbon composite as the structural member of the turbine blade) • Infrastructure • Offshore Drilling • Mining

PERFORMANCE PROPERTIES: • High Stress & Stiffness • Corrosion Resistant • High Fiber Volume • Extremely Low Void Content • Locked In Filament Alignment.

Property data for a 3.2 mm flat plate.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2350 MPa
Tensile Modulus 140 GPa
Compressive Strength 1450 MPa
Compressive Modulus 130 GPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zoltek™ PX35 Pultruded Carbon Fiber/Epoxy Profile
Solvay Thornel® P-120 Carbon Fiber/Epoxy Advanced Composite System
Solvay Thornel® P-75 Carbon Fiber/Epoxy Advanced Composite System
Hexcel® HexTow® IM6 Carbon Fiber - Epoxy Composite
Hexcel® HexTow® AS7 Carbon Fiber - Epoxy Composite

PZOL843 / 232318

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.