PBN is a high purity (99.995%), non-porous, ceramic material grown via a Chemical Vapor Deposition (CVD) process. The material has anisotropic properties due to its planar crystal structure. PBN exhibits high thermal conductivity along its crystal planes (“a” direction) and good thermal insulation through its crystal planes (“c” direction). Applications: - Crystal Growth, including GaAs and InP
- LEC, VGF and Bridgman crucibles
- MBE crucibles and furniture
- SUMO crucibles
- OLED crucibles and effusion cell hardware
- Heating elements
information provided by Morgan Advanced Materials |