MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) BLUESIL™ RTV 3625 Hi-Pro Blue Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: BLUESIL™ RTV 3625 is a low viscosity, 25 Durometer (Shore A), two component, tin catalyzed, room temperature curing silicone elastomer. It is designed as a high strength elastomer with good cured rubber properties, long library life and accurate detail reproduction. BLUESIL™ RTV 3625 can be catalyzed with BLUESIL™ Hi-Pro Green or fast setting BLUESIL ™ Hi-Pro Blue.

Applications:

  • Casting of polyester or polyurethane resins for figurine, giftware and decorative accessories
  • Architectural and furniture parts and accessories
  • Statuary and collectibles

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/cc
Viscosity 40000 cPPart A, Base Component
 60000 cPMixed
Linear Mold Shrinkage 0.0040 cm/cm
@Time 86400 sec
 0.0060 cm/cm
@Time 25200 sec
Storage Temperature 24.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 27ASTM D2240
Tensile Strength 620 psiASTM D412
Elongation at Break 390 %ASTM D412
Tear Strength 120 pliASTM D624, Die B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 168 hour
@Temperature 24.0 °C
50% RH
Shelf Life 18.0 Month
 
Descriptive Properties
ColorWhitePart A, Base Component
Mix Ratio10:1A:B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 3120 RTV SILICONE RUBBER
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Fast Cure Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 1556 B Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 1597 Silicone Rubber
Elkem (Bluestar Silicones) BLUESIL™ RTV 3165 A&B Silicone Rubber

PBLUST057 / 191033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.