General purpose extrusion grade for wire jacketing, tubing, rods, slabs and centrifugal casting. ASHLENE 831 meets FDA requirements and is therefore also suitable for film extrusion and co-extrusion applications. Data provided by the manufacturer |
Polyamide 6; Ashley Polymers, Inc. |