MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Pocan® B 1305 000000 PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: PBT, non-reinforced, General purpose grade

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.020 cm/cmPlaque 60 x 60 x 2mm; ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cmPlaque 60 x 60 x 2mm; ISO 294-4
Melt Flow 47 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break >= 10 %Nominal, 50 mm/min; ISO 527-1,-2
Elongation at Yield 9.0 %50 mm/min; ISO 527-1,-2
Tensile Modulus 2800 MPa1 mm/min; ISO 527-1,-2
Flexural Yield Strength 80.0 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Strain at Yield 6.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 90.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
 125 kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched 150 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 180 kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.019
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VTest solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point 225 °C10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi) 65.0 °CMethod Af; ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °CMethod Bf; ISO 75-1,-2
Flammability, UL94 HB
@Thickness 0.750 mm
UL Yellow Card
Glow Wire Flammability Index 750 °C
@Thickness 2.00 mm
IEC 60695-2-12
Shrinkage, MD 0.30 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
Shrinkage, TD 0.30 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °CPlaque 60 x 60 x 2mm
Mold Temperature 80.0 °CPlaque 60 x 60 x 2mm
Hold Pressure 60.0 MPaPlaque 60 x 60 x 2mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Pocan® B 1505 000000 PBT
Envalior Pocan® B 1205 HR 000000 PBT
Envalior Pocan® B 1205 XF 000000 PBT
Lanxess Pocan® B 700 000000 PBT
Envalior Pocan® S 1506 000000 PBT

PLANW9002 / 208389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.