MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMT Materials HYTAC® LP Syntactic Plug Assist System for Heavy-Gauge Thermoforming
Categories: Polymer; Thermoset; Epoxy

Material Notes: HYTAC-LP is a new epoxy syntactic plug assist system aimed at providing heavy gauge thermoformers with a durable, lightweight, low thermal conductivity, castable system that reduces large plug costs while increasing performance. HYTAC-LP will result in improved thickness control and more consistent quality of the final part. HYTAC-LP can also reduce sticking of difficult-to-process polymers.

HYTAC-LP is a two-part system consisting of a core of partially-cured epoxy coated large, hollow composite spheres and a skin of thick, non-sloughing syntactic foam.

Low Thermal Conductivity and Specific Heat: The syntactic foam structure of HYTAC-LP maintains the low thermal conductivity desired in a plug assist material.

Dimensionally Stable up to 176°C/350°F

Low Cost: The system is about half the cost of similar solid syntactic foam plugs.

Lightweight: This increases the life of capital equipment due to reduced wear and tear on moving parts.

Easily Formed or Machined: HYTAC-LP may be cast to near net shape and/or machined using conventional equipment.

Applications: HYTAC-LP now makes it possible for heavy gauge thermoforming applications to realize the same material distribution/sheet thickness reductions and energy savings as are expected in thin-gauge thermoforming. The exterior skin of the plug, the performance portion of the plug can be formulated with a variety of HYTAC materials to meet specific, application needs.

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Wollite 30 Insulating Castable
Pyrotek Wollite 37 Insulating Castable
Pyrotek Valcor® G-AZ Pre-Cast Shapes
Pyrotek Valcor® G Pre-Cast Shapes

PCMT010 / 93144

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.