MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymer Resources PRL TP-GFMF3 Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: TP (polybutylene terephthalate) is a semi-crystalline engineering thermoplastic material that offers very good chemical resistance with high levels of mechanical and thermal properties. Polybutylene terephthalate has good dimensional stability and is unaffected by ambient humidity. This semi-crystalline thermoplastic also has low friction and resistance to abrasion.

Information provided by Polymer Resources.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 in/in
@Thickness 3.17 mm
ASTM D955
Melt Flow 8.0 - 20 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14000 psi
@Thickness 3.17 mm
ASTM D638
Tensile Strength, Yield 14000 psi
@Thickness 3.17 mm
ASTM D638
Flexural Strength 22000 psi
@Thickness 3.17 mm
2.00 inch span; ASTM D790
Flexural Modulus 1.00e+6 psi
@Thickness 3.17 mm
ASTM D790
Izod Impact, Notched 1.00 ft-lb/in
@Thickness 3.17 mm,
Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 405 °F
@Thickness 3.17 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 390 °F
@Thickness 3.17 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 475 - 525 °F
Rear Barrel Temperature 470 - 490 °F
Middle Barrel Temperature 480 - 500 °F
Front Barrel Temperature 490 - 510 °F
Mold Temperature 160 - 200 °F
Drying Temperature 240 - 250 °F
Dry Time 3.00 - 4.00 hourRecommended
 <= 8.00 hourMaximum
 
Descriptive Properties
FeaturesHigh heat resistance, RoHS compliant.
FormPellets
Processing MethodInjection molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYQ285 / 277907

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.