MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite Sumikon® X655 Phenolic Novolac
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Mineral/Glass Filled

Material Notes: SUMIKON® X655 is a glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and high electrical insulation properties.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.09 g/ccJIS K 6911
Water Absorption 0.030 %JIS K 6911
Linear Mold Shrinkage 0.0011 in/inJIS K 6911
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 75.0 MPaJIS K 6911
Flexural Strength 205 MPaJIS K 6911
Flexural Modulus 27.5 GPaJIS K 6911
Compressive Strength 250 MPaJIS K 6911
Charpy Impact, Notched 3.50 kJ/m²JIS K 6911
 
Electrical PropertiesOriginal ValueComments
Insulation Resistance 2.00e+10 ohmAfter boiling; JIS K 6911
 8.00e+11 ohmAs mold; JIS K 6911
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 18.0 µm/m-°CTMA
Deflection Temperature at 1.8 MPa (264 psi) 230 °CJIS K 6911
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Vyncolit® X651 Phenolic Novolac
Sumitomo Bakelite Vyncolit® W5016 Phenolic Novolac
Sumitomo Bakelite Vyncolit® X7306 Phenolic Novolac
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate
Norplex-Micarta ShotBlocker NP523 Phenolic Glass Laminate Sheet

PSUMIT483 / 194288

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.