MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-SEAL 1287 Conductive Elastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Rubber or Thermoset Elastomer (TSE)

Material Notes: Conductive Fluorosilicone EMI/EMP Gasket. This material is silver-plated-aluminum-filled fluorosilicone elastomer which provides pressure and environmental sealing as well as high levels of EMI shielding. It is one of the more corrosion resistant silver-based elastomers, and is recommended where both salt spray and jet fuel environments are present.

Molded and Extruded

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.75 - 2.25 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 63 - 77ASTM D2240
Tensile Strength at Break >= 180 psiASTM D412
Elongation at Break 60 - 260 %ASTM D412
Tear Strength 6.13 kN/mASTM D624
Compression Set <= 30 %
@Temperature 100 °C,
Time 252000 sec
ASTM D395 Method B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.012 ohm-cmwithout psa; MIL-DTL-83528
 0.015 ohm-cmPost Tensile Set; MIL-G-83528 Para.4.6.9
Shielding Effectiveness >= 55 dB
@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
 >= 75 dB
@Frequency 4.00e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 90 dB
@Frequency 1e+10 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 95 dB
@Frequency 2.00e+9 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
 >= 100 dB
@Frequency 5.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
 >= 110 dB
@Frequency 1e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -55.0 °CFlex TR10; ASTM D1329
 
Descriptive Properties
BinderFluoro-silicone
EMP Survivability >0.9 kA / inMIL-DTL-83528 Para.4.6.16
FillerAg/Al
GradeMilitary-Aerospace
Heat Aging <0.015 ohm-cmMIL-DTL-83528 Para.4.6.15
Type DMIL-DTL-83528
Vibration Resistance, After<0.012 ohm-cmMIL-DTL-83528 Para.4.6.13
Vibration Resistance, During<0.015 ohm-cmMIL-DTL-83528 Para.4.6.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit Consil®-C 875 Silver-Copper Filled Silicone Elastomer
Precision Polymer Engineering S70S Conductive Silicone Rubber
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer
Parker Chomerics CHO-SEAL 1278 Conductive Elastomer
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer

PCHOME126 / 28348

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.