MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kingfa CPA-6 Toughened PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes:
    Features:
  • High impact
  • Low tendency to wrap

    Applications:
  • Injection molding
  • Sport appliance
  • Automobile parts
  • Power tools

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
@Temperature 23.0 °C
ASTM D792
Water Absorption 0.60 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
@Temperature 23.0 °C
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 108ASTM D785
Tensile Strength at Break 45.0 MPa10mm/min; ASTM D638
Elongation at Break >= 50 %10mm/min; ASTM D638
Flexural Strength 63.0 MPa2mm/min; ASTM D790
Flexural Modulus 1680 MPa2mm/min; ASTM D790
Izod Impact, Notched 780 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 208 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °C
Rear Barrel Temperature 225 - 245 °CStart Point: 230°C
Middle Barrel Temperature 250 - 270 °CStart Point: 255°C
Front Barrel Temperature 260 - 280 °CStart Point: 265°C
Melt Temperature 255 - 285 °CStart Point: 265°C
Mold Temperature 50.0 - 70.0 °CStart Point: 60°C
Drying Temperature 90.0 - 110 °C
@Time 14400 - 21600 sec
Pre-dry
 
Descriptive Properties
Injection SpeedModerate to High

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa PA66-C111 Toughened PA66
BASF Ultramid® 8202 PA6 (Dry)
Eurotec® Tecomid® NB40 NL IL PA6, impact modified, natural
BASF Nypel® 6030G HS BK 30% Glass Filled PA6 (Dry)
Ashley Polymers Ashlene® 180 Acetal

PKINGF027 / 104286

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.