Notes: Monprene RG-20100 series is group of high performance thermoplastic elastomer specifically designed for extruded regulated applications including food contact, toys and children’s products. Monprene RG-20160 is a low density, Medium hardness grade that complies with various US FDA and European regulations and directives for food contact and toy safety and is suitable for extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: BPA Free, Food Contact Acceptable; Good Adhesion; Good Colorability; Good Processability; Low Flow; Low Density; Low Specific Gravity; Lubricated; Medium Hardness; No Animal Derived Components; Slip; Without Fillers Uses: Consumer Applications; Cosmetic Packaging; Food Containers; Food Packaging; Food Service Applications; Kitchenware; Lids; Non-specific Food Applications; Rubber Replacement; Toys RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Extrusion Preliminary data. Information provided by Teknor Apex |