MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Pyrocast PT-60 Castable Refractory
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Pyrocast PT-60 is a ceramic fiber based insulating castable with very low thermal conductivity and excellent resistance to thermal shock.

Applications

  • Launder linings
  • Distributor pan linings
  • Ladle linings

Advantages

  • In situ casting
  • Excellent insulation characteristics
  • Does not require pre-heating

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.800 g/ccoven dried
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000600 GPa
Compressive Strength 0.800 MPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.210 W/m-K
@Temperature 800 °C
Maximum Service Temperature, Air 1320 °C
Shrinkage 0.20 %
@Temperature 815 °C,
Time 18000 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast AR-S Castable Refractory
Pyrotek Pyrocast AR70 Low-Density Refractory Castable
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrotek Pyrocast XL Small Component Refractory

CPYRO134 / 1856

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.