Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel. Meets FDA Dry Bulk Food Regulation Title CFR, Paragraph 175.300. Socomore acquired the Aeroglaze® and Chemglaze® product lines from Lord in September 2016. |