Notes: Monprene CP-37185 is a general purpose thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-37185 is a high density, high hardness grade suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Filled; High Density; High Specific Gravity; High Hardness; Medium Flow; Slip Uses: Consumer Applications; Gaskets; Handles; Kitchenware; Safety Equipment; Sporting Goods; Toothbrush Handles; Writing Instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |