MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics WIN-SHIELD™ P (Polycarbonate) EMI Shielded Window
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Optical Grade

Material Notes: Description: Parker Chomerics display windows and filters are available in various plastic materials, including polycarbonate, acrylic and cast polycarbonate. A unique feature of Parker Chomerics window products is the capability to laminate together multiple substrates allowing for a fully customized design. This process allows for the incorporation of specialty materials for EMI shielding, light control, polarization and other value added features. The use of polycarbonate or acrylic offers the most flexibility in application design.

Surface Finish Option: Clear, Semi-Gloss, Matte Hardcoats, & Anti-Reflective Surfaces

Design Options: Screen Printing, Heat Shielding, Privacy Filters & Other Specific Designs are Available.

Typical Applications: Ruggedized Displays, Military, Aerospace, Industrial Applications, Medical, Test Instruments and EMI Shielding for Touch Screens

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 510 - 12700 microns
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 70
 
Electrical PropertiesOriginal ValueComments
Shielding Effectiveness 73 - 105 dB
@Frequency 1e+8 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Minimum Service Temperature, Air -55.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 63 - 85 %Mesh Only

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
COI Ceramics Nextel™ AS-N720 Oxide Ceramic Matrix Composite, Aluminosilicate
Clariant Renol PCSP0015 Polycarbonate, Carbon Fiber Filled
Clariant Renol PCSP0004 Polycarbonate Alloy
Chi Mei Wonderloy® PC-345 PC/ABS Alloy
Chase Plastics CP Pryme® PC310R Polycarbonate, 10% Glass Fiber Reinforced, Recycled Content

PCHOME276 / 130986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.