MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Process Technologies Inc FKM/Metal - Metal Detectable Sanitary Gasket
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: FKM/Metal is FDA compliant. This material provides high acid and temperature resistance. It does not have strong Base resistance and performs very poorly when used with Ketones. FKM/Metal is not recommended for continuous use in SIP procedures.

Information provided by Process Technologies Inc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 204.44 °C
Minimum Service Temperature, Air -28.89 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Compatibility for ChemicalsAcetoneNot Recommended
 AmmoniaNot Recommended
 Hydrochloric AcidExcellent
 Hydrofluoric AcidLimited
 Hydrogen PeroxideGood
 Isopropyl AlcoholExcellent
 Nitric AcidExcellent
 Phosphoric AcidExcellent
 Sodium HydroxideGood
 Sodium HypochloriteExcellent
 Steam to 400ºF (204ºC)Not Recommended
 Sulfuric AcidExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Seals Eastern 5725 Fluorocarbon-Elastomer
Cri-Tech FDA-615 FKM Fluoroelastomer, Durometer 61A
Seals Eastern 5722 Fluorocarbon-Elastomer
Chemours Viton® A-700 Fluoroelastomer (FKM)
Chemours Viton® F-601C Fluoroelastomer (FKM)

PPTI12 / 138124

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.