MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Partially Aromatic, Glass Filled; Nylon, Aromatic

Material Notes: PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved heat resistance. Delivered in natural mode and in the full RAL color scale.

Information Provided by Plastcom spol. s r.o.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccSTN EN ISO 1183-1
Filler Content 35 %
Linear Mold Shrinkage 0.0030 cm/cmSTN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0080 cm/cmSTN EN ISO 294-4
Melt Flow 3.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
STN EN ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPaSTN EN ISO 527-2
Elongation at Break 2.0 %STN EN ISO 527-2
Tensile Modulus 11800 MPaSTN EN ISO 527-2
Flexural Strength 310 MPaSTN EN ISO 178
Flexural Modulus 9900 MPaSTN EN ISO 178
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 95.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -20.0 °C
STN EN ISO 179
 16.0 kJ/m²
@Temperature 23.0 °C
STN EN ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+15 ohm-cmSTN 34 6460
Surface Resistance 8.00e+13 ohmSTN 34 6460
Dielectric Strength 20.0 kV/mmSTN EN 60243-2
Comparative Tracking Index 600 VSTN EN 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 295 °CSTN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 275 °CSTN EN ISO 75-2 (A)
Vicat Softening Point 275 °CSTN EN ISO 306
Flammability, UL94 HB
Glow Wire Flammability Index 650 °C
@Thickness 3.00 mm
STN EN 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 310 - 340 °C
Mold Temperature 90.0 - 120 °C
Drying Temperature 120 °C
@Time 14400 sec
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Heat Stabilized
Radici Radilon® CST (dry) Copolyamide 6 semiaromatic
Envalior Novamid® 2620A PA6/6T
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Dry)
BASF Ultramid® T 4381 LDS 10/25% Glass/Mineral Filled PA6/6T (Conditioned)

PPLACO538 / 140939

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.