MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Grupo Repol Dinalon® B2S35 V2-7035 PA6 High Viscosity, V2 Halogen Free, RAL 7035
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes: Mechanical properties for Dry As Molded samples

Information provided by Grupo Repol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.16 g/ccISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %Karl-Fischer; ISO 15512/A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPaISO 527
Elongation at Yield 4.0 %ISO 527
Tensile Modulus 3.30 GPaISO 527
Flexural Strength 80.0 MPaISO 178
Flexural Modulus 1.80 GPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CISO 75/A
Vicat Softening Point >= 200 °C50N; ISO 306
Flammability, UL94 V-2
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Omni Plastics OmniTech™ PA6/6,6 V2 125 IM8 Flame Retardant
Grupo Repol Dinalon® B1X25 V0 PA6 V0 Red Phosphorus and Halogen Free
Aluminum 5052-H34
5754-H22 Aluminum

PGRU130 / 43320

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.