Hostalen GM 9310 C black is a electrically conductive high density polyethylene (HDPE), black colored similar RAL 9004 with high melt viscosity for pipes, fittings and sheets for application in explosion-proof areas. The product provides good long term hydrostatic strength. Applications: IndustrialInformation provided by LyondellBasell. |