MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
USI Corporation FREVA™ SEG60 Glass Fiber Reinforced Composited Sheet
Categories: Other Engineering Material

Material Notes: Description:
  • USI Glass fiber reinforced composited sheet FREVATM SEG60 is a good replacement of ceramic sheet applying to heat and electrical insulation.
  • FREVATM SEG60 is a new organic-inorganic green material that is halogen-free, formaldehyde-free, toluene-free, and heavy metal free. When it is burned, most of the emission is water vapor with very low smoke.
  • FREVATM SEG60composited by non-halogen flame retardant polymer, which can resist >1000 °C blaze flame for more than 60 minutes with a thickness of 0.75mm. According our test result, FREVATM SEG60 can achieve a UL-94 V0 rating at 0.75 mm.
  • Standard roll widths: 1200mm
  • Standard roll length: 50m, 100m, 200m

Information provided by USI Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.60 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 14.7 MPa0.75; ASTM D638
Elongation at Break 10 %
@Thickness 0.750 mm
ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 4.00 kV/mm
@Thickness 3.00 mm
ASTM D149
Dielectric Breakdown 12100 V
@Thickness 3.00 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.50 W/m-K
@Thickness 6.00 mm
ISO 22007-2
Flammability, UL94 V-0
@Thickness 0.600 mm
 
Descriptive Properties
Thermal Resistance0.4°C/W6mm, ISO 22007-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PUSIC043 / 285411

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.