MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® U 2500 HTR Two-Component Polyurethane Encapsulant
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Loctite Stycast U 2500 HTR provides the following product characteristics:
  • Low viscosity
  • Low modulus
  • High temperature resistance
  • Excellent wetting properties

Cure: Room Temperature or Heat Cure

Application: Potting, Encapsulant

Typical Assembly Applications: Transformers, PCB's and other insulating applications

Loctite Stycast U 2500 HTR flexible polyurethane encapsulant is formulated to have low viscosity and excellent wetting properties allowing complete impregnation of either small slightly wound coils or large castings. It can also be used to replace silicones. Loctite Stycast U 2500 HTR has a higher service temperature than standard polyurethane materials.

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccPart B
 1.42 g/ccPart A
Moisture Absorption 0.600 %
@Temperature 24.0 °C,
Time 86400 sec
 0.600 %
@Temperature 100 °C,
Time 3600 sec
Viscosity 5.0 cPPart B
 8000 cPMixed
 12500 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
Tensile Strength 4.00 MPa
Elongation at Break 66 %
Modulus of Elasticity 0.0100 GPa
Adhesive Bond Strength 6.00 MPaLap Shear Strength, Al to Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.70e+12 ohm-cm500 Volts
Surface Resistance 1.90e+13 ohm
Dielectric Constant 6.0
@Frequency 1e+6 Hz
 7.0
@Frequency 50 Hz
 7.1
@Frequency 1000 Hz
Dissipation Factor 0.030
@Frequency 1000 Hz
 0.050
@Frequency 50 Hz
 0.050
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 134 µm/m-°C
@Temperature >=-50.0 °C
Above Tg
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg -50.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 60.0 °C
Option 2, Post Cure: 2 hours @ 100 to 120°C
 24.0 hour
@Temperature 25.0 °C
Option 1, Post Cure: 2 hours @ 100 to 120°C
Pot Life 240 min
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceAmberComponent B, Hardener
 BlackComponent A, Resin
Mix Ratio, by Weight100 : 7.6Component A : Component B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7962 / 255446

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.