MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AlphaGary Dural 202/3 CLEAR 0003 Full Rigid Polyvinyl Chloride Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: Dural is a full rigid PVC compound series that offers excellent heat and dimensional stability with easy processing.
Wide range of medical and general purpose applications

Alphagary is part of Orbia.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %Clear; thickness not specified
 
Descriptive Properties
DEHP FreeYes
Phthalate FreeYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Dural® Aluminum /Copper/Magnesium Alloy
Fainplast Compounds MRK 267 Medical Rigid PVC, Injection Molding
AlphaGary Dural 205JB CLEAR 0003 Full Rigid Polyvinyl Chloride Compound
Fainplast Compounds MRT 168 Medical Rigid PVC, Injection Molding
AlphaGary Dural 725C CLEAR 0003 Full Rigid Polyvinyl Chloride Compound

PGARY9917 / 140703

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.