MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Domo TECHNYL® C 536XT PA6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Extruded

Material Notes: Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.

Benefits: The product offers a good processing behavior, high impact resistance even at low temperature and high barrier properties especially to fluids such as fuels and oils, as well as a high toughness.

Available in: Europe and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This grade is particularly recommended for use in applications such as tanks or pipes.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccISO 1183/A
Water Absorption 1.27 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Viscosity 220 cP
@Shear Rate 1000 1/s,
Temperature 270 °C
 1050 cP
@Shear Rate 100 1/s,
Temperature 270 °C
 2200 cP
@Shear Rate 10 1/s,
Temperature 270 °C
Linear Mold Shrinkage 0.010 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0206 cm/cm
Linear Mold Shrinkage, Transverse 0.0207 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 47.0 MPaISO 527 Type 1A
Tensile Strength, Yield 54.0 MPaISO 527 type 1 A
Elongation at Break 55 %ISO 527 Type 1A
Elongation at Yield 4.0 %ISO 527 type 1 A
Tensile Modulus 2200 MPaISO 527 Type 1A
Flexural Modulus 1950 MPaISO 178
Izod Impact, Notched (ISO) 66.0 kJ/m²ISO 180/1eA
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 16.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 76.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 220 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °CISO 75/Af
 
Processing PropertiesOriginal ValueComments
Feed Temperature 200 - 220 °C
Adapter Temperature 210 - 230 °C
Die Temperature 215 - 230 °C
Head Temperature 220 - 230 °C
Screw Cooling Temperature 210 - 230 °C
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 80.0 °C
@Time 28800 sec
dew point -35°C
Moisture Content <= 0.080 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® ET3117 Polycarbonate
Domo TECHNYL® C 502XT PA6, DRY
Domo TECHNYL® C 536XT PA6, Conditioned
Overview of materials for Nylon 6, Extruded
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded

PRHOD814 / 138045

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.