Hostacom TYC712N GRY high melt flow, 1,900 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an excellent balance of processability, rigidity, and impact resistance. It is typically used for assorted automotive interior trim components.Information provided by LyondellBasell. |