System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LG Chemical LUMAX EU5300 PBT+ASA+GF30%, Injection Molding
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
PBT + ASA Blend, Glass Fiber Reinforced
Material Notes:
Low Warpage, Good surface
Application: E&E, Automotive
Information provided by LG Chemical
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.46
g/cc
ASTM D792
Water Absorption
0.060 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow
0.0030
-
0.0050
cm/cm
ASTM D955
Melt Flow
13
g/10 min
@Load 2.16 kg,
Temperature 250 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
1250
kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Elongation at Break
2.0 %
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Strength
177
MPa
@Thickness 6.40 mm
5mm/min; ASTM D790
Flexural Modulus
84000
kg(f)/cm²
@Thickness 6.40 mm
5mm/min; ASTM D790
Izod Impact, Notched
8.00
kg-cm/cm
@Thickness 3.20 mm
ASTM D256
Thermal Properties
Original Value
Comments
Melting Point
223
°C
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi)
195
°C
@Thickness 6.40 mm
Unannealed; ASTM D648
Flammability, UL94
HB
@Thickness 1.60 mm
Processing Properties
Original Value
Comments
Rear Barrel Temperature
240
-
260
°C
Middle Barrel Temperature
240
-
260
°C
Front Barrel Temperature
245
-
265
°C
Nozzle Temperature
245
-
265
°C
Melt Temperature
240
-
260
°C
Mold Temperature
40.0
-
80.0
°C
Drying Temperature
120
°C
@Time 14400 - 21600 sec
Moisture Content
<= 0.020 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
INEOS Styrolution Luran® S 757G ASA
Ravago Manufacturing Americas Hysun 677UVG15 ASA, Acrylonitrile Styrene Acrylate, 15% Glass Filled, UV stabilized, DAM
Ravago Manufacturing Americas Hysun 677G30 ASA, Acrylonitrile Styrene Acrylate, 30% Glass Filled, DAM
Ravago Manufacturing Americas Hysun 677G20 ASA, Acrylonitrile Styrene Acrylate, 20% Glass Filled, DAM
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
PLHCHEM9732 / 239256
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.