MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotchkote™ SG 527 Epoxy Metal Repair
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Metal Repair SG 527 is a specially packaged rapid curing synthetic metal repair compound for on site repairs to metal components such as leaking pipes, tanks, ducts, and radiators.

Product Features:

  • Simple to use, only requiring simple hand mixing to activate reaction between the concentrically packed components
  • Designed for application by gloved hand, putty knife or spatula
  • Can be applied to any damaged metal surface, plus glass, fiberglass and other composite surfaces
  • Designed for rapid repairs to cracked casting, leaking pipes, tanks, flanges etc. minimizing downtime
  • Excellent adhesion to correctly prepared metal surfaces.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 3250 psi
Compressive Strength 5000 psi
Shear Strength 650 psiTensile Shear Adhesion, on a grit blasted steel
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 40.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hourHard Dry for machining
 2.00 hourFull Cure
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotchkote™ EG 503 Epoxy Metal Repair
Abatron Ferrobond-P™ Steel-Filled, Structural Adhesive Putty; Paste
Overview of materials for Epoxy, Cast, Metal Filled
Polynt DISTITRON® VE 100 ST Epoxy Resin Based Vinyl Ester
Polynt EPOVIA OPTIMUM® KRF 1001 TAS Bisphenol-A Epoxy Resin

PMM35298 / 170045

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.