The EC/PA series is a material solution for applications with requirements on electrical conductivity. The materials come with low resistivity and adhesion to polyamides and polypropylene. The compounds are halogen-free according to IEC 61249-2-21. They are available in black colors only. Processing Method: Injection Molding, Extrusion Color / RAL DESIGN: Typical applications: - Electric and electronic components
- Stylus
- Grip applications
- Grommets
- Flexible conductors
- ESD protection
- Dead man's switches
- Sensors
Material advantages:- Electrical conductivity
- Low resistivity
- Adhesion to PA6 and PA6.6
- Soft, non-sticky haptic
- Adhesion to PP
- Halogen-free (according to IEC 61249-2-21)
- In-process recycling possible
Information provided by Kraiburg TPE |