MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 933-1 Moisture Resistant Chip Encapsulant
Categories: Polymer; Thermoset; Epoxy; Filled/Reinforced Thermoset

Material Notes: TRA-BOND 933-1 one component, highly filled, electrically insulating epoxy encapsulant is designed for encapsulating microelectronic chips. This epoxy provides excellent environmental and mechanical protection. TRA-BOND 933-1 encapsulant exhibits a longer work life and a lower moisture sensitivity than the anhydride-cured systems. The low coefficient of thermal expansion minimizes stress effects on components and wiring during thermal shock tests.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.10 g/ccCured
Water Absorption 0.11 %
Viscosity 360500 cP
@Temperature 25.0 °C
After mixing
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) 55 ppm
Ionic Impurities - Cl (Chloride) 300 ppm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 92
Adhesive Bond Strength 2500 psiLap shear, alum to alum, 2 hrs @ 150°C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
@Temperature 100 °C
Dielectric Constant 6.1
Dielectric Strength 1000 V/mil
Dissipation Factor 0.0070
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 µm/m-°CBelow Tg
 100 µm/m-°CAbove Tg
Thermal Conductivity 1.00 W/m-K
@Temperature 121 °C
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -60.0 °C
Glass Transition Temp, Tg 124 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 125 °C
 30.0 min
@Temperature 150 °C
 
Descriptive Properties
Color Black
Water Extract Conductivity umhos/cm 290
Weight Loss % 0.67At 300°C
Working Life, months 2At 25°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRAC202 / 71130

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.