TRA-BOND F194 is a high strength, anaerobic adhesive system designed for use in fiberoptic terminations or any applications requiring bond lines below .005". This system bonds well to all types of glass, metals and ceramics. This 100% solids adhesive is low viscosity and gels quickly at room temperature. TRA-CON supplies TRA-BOND F194A in syringes and Primer F194B in glass vials for easy application. Abrade clean and dry all substrates. Brush Primer F194B on to one substrate. Apply TRA-BOND F194A to second substrate. Press together and apply pressure for 1 to 2 minutes. Information provided by Tra-Con Inc. |