MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecapeek® XP-98 Medical Compression Molded PEEK Compound, 30% Carbon Fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.

TECAPEEK is a high-performance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.

Typical Applications:

  • Bearings and Bushings
  • Down-hole instrumentation
  • Wear Rings
  • Ball Valve Seats
  • Electrical Components
  • Back-up and V-Rings
  • Piston Rings and Rider Bands

Information provided by Ensinger Special Polymers, Inc.

Vendors: Ensinger Special Polymers, Inc. provides consistent, high quality compression molded stock shapes of engineering thermoplastics. Common shapes include rings, rods, plates, tubes, and discs. Large diameter rings up to 90" OD are available.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccASTM D792
Filler Content 30 %
Water Absorption 0.050 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 102ASTM D785
Hardness, Shore D 93ASTM D2240
Tensile Strength 18300 psiASTM D638
Elongation at Break 2.2 %ASTM D638
Tensile Modulus 1.40e+6 psiASTM D638
Flexural Strength 30500 psiASTM D790
Flexural Modulus 1.60e+6 psiASTM D790
Flexural Strain at Break 1.7 %ASTM D790
Compressive Strength <= 26000 psiASTM D695
Compressive Modulus 600000 psiASTM D695
Shear Strength 12100 psiASTM D732
Izod Impact, Notched 1.03 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance <= 10000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.8 µin/in-°FASTM E831
Melting Point 649 °FDSC
Heat Distortion Temperature >= 459 °FASTM D648
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Tecapeek® XP-98HT Compression Molded PEEK HT, 30% Carbon Fiber
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber
Ensinger Tecapeek® XP-99 Compression Molded PEEK Compound, Bearing Grade Material with 7% Graphite, 8% PTFE, and 15% Carbon Fiber
Ensinger Tecapeek® XP-109 Compression Molded PEEK Compound, 30% Carbon Fiber with 15% PTFE

PENSIN917 / 140790

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.