MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nurel Engineering Polymers Promyde® B30 P2 G50 PA 6, Dry, 50% Glass Reinforced, Injection Molded and Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Characteristics: Promyde B30 P2 G50 is distinguished by high mechanical strength, hardness, rigidity, thermo stability (melting point 220ºC), and resistance to hot lubricants and water. Parts made from Promyde B30 P2 G50 have particularly high dimensional stability and creep strength.

Applications: Promyde B30 P2 G50 is used in a wide range of applications where a combination of mechanical properties and thermal resistance is needed. Glass-fiber reinforced grades are suitable for housings, supports, industrial articles and electrical insulating parts.

Information provided by Nurel Engineering Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
Moisture Absorption 1.50 %50%, rh; ISO 62
Water Absorption at Saturation 4.5 %in water; ISO 62
Viscosity Test 145 cm³/gViscosity Number; ISO 307
Linear Mold Shrinkage, Flow 0.0030 - 0.0035 cm/cm
Linear Mold Shrinkage, Transverse 0.0040 - 0.0045 cm/cm
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 275 °C
[cm3/10 min], MVR; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 215 MPa50 mm/min; ISO 527-1/-2
Elongation at Break 3.0 %50 mm/min; ISO 527-1/-2
Tensile Modulus 15600 MPa1 mm/min; ISO 527-1/-2
Flexural Strength 340 MPa2 mm/min; ISO 178
Flexural Modulus 14000 MPa2 mm/min; ISO 178
Charpy Impact Unnotched 95.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 19.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+13 ohmIEC 60093
Dielectric Constant 4.2
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 500 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 13.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-1/-2
Melting Point 222 °CDSC 10°C/min; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 215 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 215 °CISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 - 290 °Cinjection molding
Mold Temperature 40.0 - 80.0 °C
Drying Temperature <= 80.0 °C
Dry Time 4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Reny® 1022H Polyamide
Niche Polymer PA6GF50BK Nylon 6, 50% Glass Fiber Filled
Omni Plastics OmniLon™ PA6 GR50 Nylon 6, 50% Glass reinforced
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber
NYCOA 27/300I Glass Filled Nylon 6

PNUREL054 / 183419

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.