Product Description: Metal Plating Grade. Characteristics: High impact, Low gel, Metal plating Availability: Asia Pacific; Europe; North America Features: High Flow; High Impact Resistance; Low Gel; Platable Agency Rating: EC 1907/2006 (REACH) RoHS Compliance: RoHS Compliant UL File Number: E162823 Processing Method: Injection MoldingInformation provided by Formosa Chemicals & Fiber Corporation |