MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days for the Scotch-Weld epoxy adhesive 2216 Translucent B/A to minutes and hours. Final shear and peel strengths remain similar or even slightly improved compared to the Scotch-Weld epoxy adhesive 2216 Translucent.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 2000 - 8000 cPBase, RVF #7 spindle, 20 rpm @ 27°C
 22000 - 33000 cPAccelerator, RVF #7 spindle, 20 rpm @ 27°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55ASTM D2240
Tensile Strength at Break 17.2 MPaASTM D882
Elongation at Break 150 %ASTM D882
Shear Strength 25.0 psiOverlap, Polypropylene
 200 psiOverlap, +3M Primer 3901
 250 psiOverlap, Glass, Borosilicate
 420 psiOverlap, Acrylic
 460 psiOverlap, ABS
 500 psiOverlap, PVC
 700 psiOverlap, Wood, Fir
 700 psiOverlap, Polycarbonate
 1200 psiOverlap, Fiberglass
 1400 psiOverlap, Sanded Aluminum
 1500 psiOverlap, Cold Rolled Steel
 2500 psiOverlap, Etched Aluminum
 150 psi
@Temperature 82.0 °C
Overlap
 190 psi
@Temperature 66.0 °C
Overlap
 400 psi
@Temperature 49.0 °C
Overlap
 2500 psi
@Temperature 21.0 °C
Overlap
 4000 psi
@Temperature -55.0 °C
Overlap
Peel Strength 2.00 pli180°
 3.00 pli180°
 3.00 pli180°
 10.0 pli180°
 35.0 pli180°
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.20e+11 ohm-cmASTM D257
Dielectric Constant 6.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 765 kV/in
@Thickness 0.762 mm
ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 112 µm/m-°C
@Temperature 5.00 - 20.0 °C
Below Tg
 190 µm/m-°C
@Temperature 65.0 - 140 °C
Above Tg
Thermal Conductivity 0.154 W/m-K
@Thickness 6.35 mm,
Temperature 44.3 °C
Glass Transition Temp, Tg 3.00 °COnset
 15.0 °CMid-Point
 
Processing PropertiesOriginal ValueComments
Cure Time 2.50 hourTime to Handling Strength
 7.00 hourFull
Tack-Free Time 2.00 hour
 
Descriptive Properties
AppearanceAmberAccelerator
 ClearBase
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
Copper, Cu; Annealed
AK Steel 316 Austenitic Stainless steel
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive

PMM34621 / 169368

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.