MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics ECOPLATE™ 5030
Categories: Metal

Material Notes: Description: ECOPLATE™ 5030 is a pure metal wire with a metallurgical composition free of defects or contaminates. When applied with the automated ECOPLATE process, it conforms to the substrate much like paint, but with the superior EMI shielding performance of solid metal. This highly engineered laminar film has low porosity and oxidation, and require no curing or further process.

Adhesion: Adhesion of the ECOPLATE™ 5030 allow is excellent with standard plastics and metals used in electronic device parts and housings. These include PC. ABS, PC/ABS, polysulfone and other thermoset or thermoplastic injection molded polymer; and aluminum, magnesium and zinc die-cast alloys. Its corrosion resistance makes ECOPLATE™ 5030 material an excellent choice for ensuring the long-term conductivity of metallic housings.

Compatibility: Following application, ECOPLATE™ 5030 material withstands low temperature solder operations, such as soldering of a shielded grounding cable onto connector back shells. The ECOPLATE™ alloy surface also functions as a replacement for plating or metallization of parts in preparation for robotic dispensing of Cho-Form® form-in-place gasketing.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.0050 ohm
@Thickness 0.0300 mm
Chomerics 95-40-5104
Shielding Effectiveness 75 dB
@Frequency 1e+10 Hz
CHO-TM-TP08
 90 dB
@Frequency 1e+8 Hz
CHO-TM-TP08
 90 dB
@Frequency 5.00e+8 Hz
CHO-TM-TP08
 90 dB
@Frequency 2.00e+9 Hz
CHO-TM-TP08
 
Thermal PropertiesOriginal ValueComments
Melting Point 270 °C
Maximum Service Temperature, Air 200 °C
 
Descriptive Properties
Adhesion5BASTM D3359-78 Method B
Alloy Ratio80/20
CompositionTin/Zinc
Film Porosity<6%
Typical Film Build0.0005 - 0.0015 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayblend® 2953 Polycarbonate + ABS Blend, Automotive Plating
Covestro Bayblend® T45 PG Polycarbonate + ABS
Trinseo PULSE™ EXT 200 PC/ABS Engineering Resin
A. Schulman Diamond ABSPC 8901P ABS/PC Plating Grade, High Impact
Acerde Tungsten

PCHOME253 / 130963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.